The C555 Concrete Moisture Meter provides fast, non-destructive preliminary moisture measurements on smooth, firm concrete to help pinpoint problem areas and determine where to place Rapid RH® L6 Smart Sensors. Built-in sensors measure ambient temperature, relative humidity and dew point.
The included On-Demand Calibrator allows fast, easy user-calibration. A NIST-traceable version, with a certificate of calibration, can also be purchased.
With its built-in ambient sensors and On-Demand Calibrator, the C555 comes with everything you need to perform the test outlined in ASTM F2659.
Relative mode can be used on other materials such as concrete block.
1-year warranty.
Use as advised in ASTM F2659
Provide a preliminary evaluation of comparative moisture conditions of concrete, gypsum cement, or other floor slabs and screeds. Good tool for testing the surface moisture in concrete.
Built-in Ambient Sensors
Measure ambient temperature, relative humidity and dew point.
Quick Readings
Capture moisture readings instantly for faster readings and results.
On-Demand Calibration
Calibrate on the go with the On-Demand Calibrator. Maintain your meter's precision without the hassle of returning it for recalibration.
Relative Measurement Mode
Measure other concrete-similar materials such as concrete blocks.
Depth Measurements
Measure moisture hotspots 0.5 inches into the concrete slab.
Press to Hold Readings
Lock in moisture readings with a single press of a button—ideal for tight corners, overhead spaces, or hard-to-reach areas. This feature is perfect for situations where the display isn't easily visible.
Twice as Accurate Compared to Leading Concrete Moisture Meters
Wagner Meters conducted an in-house case study, evaluating the accuracy of the C555 Concrete Moisture Meter against the top leading concrete moisture meter manufacturers, across nine varied and commonly used concrete mix designs in the United States. Recognizing that different concrete compositions dry and react differently, our study was designed to encompass a broad spectrum of mixes—ranging from those with fly ash and air entrainment to mixes fortified with fibers or modified with accelerators and retarders.
NIST Traceable
For an additional purchase, the C555 Concrete Moisture Meter’s calibration can be NIST certified.
Compatible with Meter Reach Extender Accessory
Pair your C555 with Wagner Meter's Meter Reach Extender for hard-to-reach spaces.

The C555 identifies potential problem areas in concrete with high RH levels, enhancing the placement of Rapid RH sensors for accurate moisture measurement. It facilitates evaluations up to ½ inches below the surface, making it a valuable tool for optimizing sensor placement and ensuring precise in situ RH testing results. The C555 can be used for non-destructive moisture evaluation, simplifying and improving the process of moisture determination in concrete.
Wagner Meters conducted an in-house case study, evaluating the accuracy of the C555 Concrete Moisture Meter against the top leading concrete moisture meter manufacturers, across nine varied and commonly used concrete mix designs in the United States.The graph provided illustrates the average moisture meter error when testing these specific mix designs. Our findings were compelling: the C555's readings were consistently closer to the benchmark oven-dry results compared to others, solidifying its status as twice as accurate as the leading concrete moisture meters.

KEY
Mix 1 - 3000 3/8-inch aggregate with fly ash and air entrainment
Mix 2 - 3000 ¾-inch aggregate with no fibers
Mix 3 - 3500 ¾-inch aggregate with accelerator
Mix 4 - 3500 ¾-inch aggregate with retarder
Mix 5 - 3500 ¾-inch aggregate with fly ash and air entrainment
Mix 6 - 4000 ¾-inch aggregate with fibers
Mix 7 - 3000 Lightweight ½-inch aggregate with fly ash POLY 997 VMA
Mix 8 - 3000 6.5 SK pea gravel pump mix POZ 80 POLY 997 VMA
Mix 9 - 3500 ¾-inch aggregate POZZ80 POLY 997
The C555 is a concrete moisture meter that can help locate problem areas in the case of a moisture-related incident. Depending on the manufacturer, you can use the C555 to determine if flooring installation is ready to install, or as a way to enhance your RH probe installation.
The C555 evaluates to ½ inch below the surface, making it a valuable tool for moisture conditions of concrete, gypsum cement, or other floor slabs and screeds. It can be used to identify pockets of high moisture levels to determine the readiness of a flooring installation depending on the manufacturer or as a supplement to the Rapid RH sensors.
Yes, the C555 can measure ambient temperature and humidity levels, helping you ensure your job site is at optimal conditions. It's like having a moisture meter and a Smart Logger all in one!
Wagner Meters conducted an in-house case study, evaluating the accuracy of the C555 Concrete Moisture Meter against the top leading concrete moisture meter manufacturers, across nine varied and commonly used concrete mix designs in the United States.The graph provided illustrates the average moisture meter error when testing these specific mix designs. Our findings were compelling: the C555's readings were consistently closer to the benchmark oven-dry results compared to others, solidifying its status as twice as accurate as the leading concrete moisture meters.

KEY
Mix 1 - 3000 3/8-inch aggregate with fly ash and air entrainment
Mix 2 - 3000 ¾-inch aggregate with no fibers
Mix 3 - 3500 ¾-inch aggregate with accelerator
Mix 4 - 3500 ¾-inch aggregate with retarder
Mix 5 - 3500 ¾-inch aggregate with fly ash and air entrainment
Mix 6 - 4000 ¾-inch aggregate with fibers
Mix 7 - 3000 Lightweight ½-inch aggregate with fly ash POLY 997 VMA
Mix 8 - 3000 6.5 SK pea gravel pump mix POZ 80 POLY 997 VMA
Mix 9 - 3500 ¾-inch aggregate POZZ80 POLY 997
Some manufacturers allow this meter to determine flooring installations or you can use a concrete moisture meter to enhance your RH probe's efficiency by locating moisture hotspots. Another way to use a C555 is for use after moisture-related issues for concrete, gypsum, brick, or other floor slabs.
No. The C555 is not calibrated or intended to be used for wood species. If you are looking for a non-damaging, accurate pinless wood moisture meter, check out Wagner Meters Orion Moisture Meters.
Wagner Meters is a trusted family-owned business that has set the standard for accuracy and reliability in the moisture measurement industry for over half a century. Our team of moisture testing experts are dedicated to helping you find the best solutions for your needs. When you choose Wagner, you're not just investing in a product—you're partnering with a company that values quality, customer care, and your success.